From: NMR and X-ray analysis of structural additivity in metal binding site-swapped hybrids of rubredoxin
 | 1HN | 15N | 1H(all) | 1HN(con)a | 15N(con) | 1H(con) |
---|---|---|---|---|---|---|
Pf metal site-swapped Cp hybrid-parentb | 0.046 | 0.279 | 0.042 | 0.049 | 0.318 | 0.043 |
Pf metal site-swapped Cp hybrid-non-parentc | - | - | - | 0.301 | 1.872 | 0.191 |
Cp metal site-swapped Pf hybrid-parent | 0.044 | 0.264 | 0.038 | 0.049 | 0.277 | 0.042 |
Cp metal site-swapped Pf hybrid-non-parent | - | - | - | 0.334 | 1.871 | 0.175 |
Cp - Pf A2K | - | - | - | 0.286 | 1.785 | 0.181 |